Sadeghi Gogheri M, Shabani M, Mirzapour E, Kasiri M, Amini K. Friction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium . JWSTI. 2016; 2 (1) :49-56
URL: http://jwsti.iut.ac.ir/article-1-75-en.html

Abstract:   (2524 Views)

In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important role in increasing hardness and tensile strength. Welding area is also has three areas. Vickers hardness is 480 times the area of welding means that the hardness in the area of the base metal of titanium and aluminum increased by 16% and 60% for titanium aluminum intermetallic compounds is created in the area is weld.

     
Type of Study: Research | Subject: Special

Add your comments about this article : Your username or email:
Write the security code in the box

Send email to the article author


© 2015 All Rights Reserved | Journal of Welding Science and Technology of Iran

Designed & Developed by : Yektaweb

تحت نظارت وف بومی آسپا-وف